Experimental, analytical, and finite element analyses of nanoindentation of multilayer PZT/Pt/SiO2 thin film systems on silicon wafers

  • C. Chima-Okereke
  • , A. J. Bushby
  • , M. J. Reece
  • , R. W. Whatmore
  • , Q. Zhang
  • Queen Mary University of London
  • Cranfield University

Research output: Other outputpeer-review

Abstract

The mechanical properties of lead zirconate titanate (PZT) multilayer systems are needed to model and design micro-electromechanical systems (MEMS) devices. Nanoindentation is a promising tool for obtaining the elastic properties of thin films. However, no means exist to obtain the elastic modulus of the lead zirconate titanate (PZT) in the multilayer system. The indentation modulus versus a/t behavior of the multilayered PZT/Pt/SiO2 film system on a silicon substrate was investigated and compared with finite element models and a new analytical solution. Six different PZT film thicknesses were indented (100, 140, 400, 700, 1500, and 2000 nm), using 5-, 10-, and 20-μm radius indenters. Good agreement was shown between the finite element analysis (FEA) and analytical solutions, and the experimental data. However the behavior of multilayer systems is complex, making deconvolution of properties difficult for films of less than a micron thick.

Original languageEnglish
Number of pages11
Edition2
Volume21
DOIs
Publication statusPublished - Feb 2006

Publication series

NameJournal of Materials Research
PublisherSpringer International Publishing AG
ISSN (Print)0884-2914

Fingerprint

Dive into the research topics of 'Experimental, analytical, and finite element analyses of nanoindentation of multilayer PZT/Pt/SiO2 thin film systems on silicon wafers'. Together they form a unique fingerprint.

Cite this