Toolbox of Advanced Atomic Layer Deposition Processes for Tailoring Large-Area MoS2 Thin Films at 150 °C

  • Miika Mattinen
  • , Jeff J.P.M. Schulpen
  • , Rebecca A. Dawley
  • , Farzan Gity
  • , Marcel A. Verheijen
  • , Wilhelmus M.M. Kessels
  • , Ageeth A. Bol
  • Eindhoven University of Technology
  • University of Michigan, Ann Arbor
  • Eurofins Materials Science

Research output: Contribution to journal › Article › peer-review

Abstract

Two-dimensional MoS2 is a promising material for applications, including electronics and electrocatalysis. However, scalable methods capable of depositing MoS2 at low temperatures are scarce. Herein, we present a toolbox of advanced plasma-enhanced atomic layer deposition (ALD) processes, producing wafer-scale polycrystalline MoS2 films of accurately controlled thickness. Our ALD processes are based on two individually controlled plasma exposures, one optimized for deposition and the other for modification. In this way, film properties can be tailored toward different applications at a very low deposition temperature of 150 °C. For the modification step, either H2 or Ar plasma can be used to combat excess sulfur incorporation and crystallize the films. Using H2 plasma, a higher degree of crystallinity compared with other reported low-temperature processes is achieved. Applying H2 plasma steps periodically instead of every ALD cycle allows for control of the morphology and enables deposition of smooth, polycrystalline MoS2 films. Using an Ar plasma instead, more disordered MoS2 films are deposited, which show promise for the electrochemical hydrogen evolution reaction. For electronics, our processes enable control of the carrier density from 6 × 1016 to 2 × 1021 cm-3 with Hall mobilities up to 0.3 cm2 V-1 s-1. The process toolbox forms a basis for rational design of low-temperature transition metal dichalcogenide deposition processes compatible with a range of substrates and applications.

Original languageEnglish
Pages (from-to)35565-35579
Number of pages15
JournalACS Applied Materials and Interfaces
Volume15
Issue number29
DOIs
Publication statusPublished - 26 Jul 2023

UN SDGs

This output contributes to the following UN Sustainable Development Goals (SDGs)

  1. SDG 7 - Affordable and Clean Energy
    SDG 7 Affordable and Clean Energy

Keywords

  • 2D materials
  • atomic layer deposition
  • electrocatalysis
  • electronics
  • low-temperature processing
  • MoS

Fingerprint

Dive into the research topics of 'Toolbox of Advanced Atomic Layer Deposition Processes for Tailoring Large-Area MoS2 Thin Films at 150 °C'. Together they form a unique fingerprint.

Cite this